Beneficiation of low-grade hematite and maghemite mixed iron ore to recover iron bearing minerals comprises e.g. providing low grade hematite and maghemite associated iron ore feed, screening the iron ore, grinding, enriching non-magnetic concentrate by rougher medium intensity magnetic separation
2023-07-15
专利权人JSW STEEL LTD (JSWS-Non-standard)
申请日期2023-07-15
专利号IN202321047804-A
成果简介NOVELTY - Beneficiation of low-grade hematite and maghemite mixed iron ore to recover iron bearing minerals comprises: (i) providing the low grade hematite and maghemite associated iron ore feed including iron, silicon dioxide, aluminum oxide and loss on ignition (LOI); (ii) screening of the low grade iron ore feed using double deck screen as beneficiated final products based on enhanced iron content; (iii) subjecting to grinding to pass at least 80% passing below 0.15 mm; (iv) processing of thus ground material of step (ii) above through medium intensity magnetic separation (MIMS) process to generate the magnetic concentrate with enhanced iron; (v) processing of MIMS non-magnetic through magnetic separation process using rougher WHIMS by subjecting to magnetic field intensity based recovery of the iron-bearing minerals as non mag concentrate; and (vi) enriching the non-magnetic concentrate through the rougher WHIMS magnetic concentrate iron grade, and magnetic separating. USE - The method is useful for beneficiation of low-grade hematite and maghemite mixed iron ore to recover iron bearing minerals. ADVANTAGE - The process utilizes hematite and mixed maghemite low grade iron ore beneficiation would enable excellent concentrate grade and higher recovery through screening, grinding to required liberation size, medium intensity magnetite separation, followed by two stage wet high intensity magnetic separation process. DETAILED DESCRIPTION - Beneficiation of low-grade hematite and maghemite mixed iron ore to recover iron bearing minerals comprises (i) providing the low grade hematite and maghemite associated iron ore feed including 52-55 wt.% iron, 14-17.3 wt.% silicon dioxide, 4-5.55 wt.% aluminum oxide and 2.29-3.4 wt.% loss on ignition (LOI); (ii) screening of the low grade iron ore feed using double deck screen to separate -40+10 mm, -10+5 mm and -5 mm and to separate the -40+10 mm and -10+5 mm as beneficiated final products based on enhanced iron content; (iii) subjecting the -5 mm size to grinding to pass at least 80% passing below 0.15 mm; (iv) processing of thus ground material of step (ii) above through medium intensity magnetic separation (MIMS) process to generate the magnetic concentrate with enhanced iron; (v) processing of MIMS non-magnetic through magnetic separation process using rougher WHIMS by subjecting to magnetic field intensity based recovery of the iron-bearing minerals as non mag concentrate; and (vi) enriching the non-magnetic concentrate of step (v) above through the rougher WHIMS magnetic concentrate iron grade, to carry out magnetic separation process using cleaner WHIMS, to generate beneficiated and recovered iron containing enriched (a) -40+10mm, (b) -10+5mm, (c) MIMS magnetic concentrate and (d) cleaner WHIMS magnetic concentrate together as final beneficiated concentrate. DESCRIPTION OF DRAWING(S) - The drawing shows a schematic view of developed beneficiation process for low grade hematite and maghemite associated iron ore.
IPC 分类号B03B-007/00 ; B03D-003/06 ; C01G-049/06 ; C21B-013/00 ; C22B-001/00
国家印度
专业领域材料科学
语种英语
成果类型专利
文献类型科技成果
条目标识符http://119.78.100.226:8889/handle/3KE4DYBR/21283
专题中国科学院新疆生态与地理研究所
作者单位
JSW STEEL LTD (JSWS-Non-standard)
推荐引用方式
GB/T 7714
PANDA D K,ATTEL U,SAH R,et al. Beneficiation of low-grade hematite and maghemite mixed iron ore to recover iron bearing minerals comprises e.g. providing low grade hematite and maghemite associated iron ore feed, screening the iron ore, grinding, enriching non-magnetic concentrate by rougher medium intensity magnetic separation. IN202321047804-A[P]. 2023.
条目包含的文件
条目无相关文件。
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。