| Preparation of elastomeric ionomer involves heating predetermined amount of halobutyl rubber for first predetermined time period to obtain mass, and adding predetermined amount of nucleophile to the mass | |
| 2023-08-01 | |
| 专利权人 | RELIANCE IND LTD (RELN-C) |
| 申请日期 | 2023-08-01 |
| 专利号 | IN202321051555-A |
| 成果简介 | NOVELTY - Preparation of an elastomeric ionomer involves: (a) heating a predetermined amount of halobutyl rubber in a preheated mixer at a first predetermined temperature under stirring at a first predetermined speed for a first predetermined time period to obtain a mass; and (b) adding a predetermined amount of a nucleophile to the mass followed by raising the temperature of mixer to a second predetermined temperature under stirring at a second predetermined speed for a second predetermined time period to obtain elastomeric ionomer. USE - Method for the preparation of an elastomeric ionomer. ADVANTAGE - The method enables to obtain elastomeric ionomer having improved strength, and self-healing properties which are required for the long life of tires. The method provides elastomeric ionomer without generating by products. The method is simple, efficient, and eco-friendly. |
| IPC 分类号 | C08K-003/00 ; C08K-003/013 ; C08L-101/00 ; C08L-023/22 ; C08L-023/26 |
| 国家 | 印度 |
| 专业领域 | 化学化工 |
| 语种 | 英语 |
| 成果类型 | 专利 |
| 文献类型 | 科技成果 |
| 条目标识符 | http://119.78.100.226:8889/handle/3KE4DYBR/21020 |
| 专题 | 中国科学院新疆生态与地理研究所 |
| 作者单位 | RELIANCE IND LTD (RELN-C) |
| 推荐引用方式 GB/T 7714 | PARASHIVA P,AMIT K,KUMAR G V,et al. Preparation of elastomeric ionomer involves heating predetermined amount of halobutyl rubber for first predetermined time period to obtain mass, and adding predetermined amount of nucleophile to the mass. IN202321051555-A[P]. 2023. |
| 条目包含的文件 | 条目无相关文件。 | |||||
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论